An All-Integrated Anode via Interlinked Chemical Bonding between Double-Shelled-Yolk-Structured Silicon and Binder for Lithium-Ion Batteries

© 2017 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

Bibliographische Detailangaben
Veröffentlicht in:Advanced materials (Deerfield Beach, Fla.). - 1998. - 29(2017), 44 vom: 21. Nov.
1. Verfasser: Liu, Yajie (VerfasserIn)
Weitere Verfasser: Tai, Zhixin, Zhou, Tengfei, Sencadas, Vitor, Zhang, Jian, Zhang, Lei, Konstantinov, Konstantin, Guo, Zaiping, Liu, Hua Kun
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2017
Zugriff auf das übergeordnete Werk:Advanced materials (Deerfield Beach, Fla.)
Schlagworte:Journal Article all-integrated electrodes binding energy double-shelled-yolk-structured lithium-ion batteries multicomponent interlinking
Beschreibung
Zusammenfassung:© 2017 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
The concept of an all-integrated design with multifunctionalization is widely employed in optoelectronic devices, sensors, resonator systems, and microfluidic devices, resulting in benefits for many ongoing research projects. Here, maintaining structural/electrode stability against large volume change by means of an all-integrated design is realized for silicon anodes. An all-integrated silicon anode is achieved via multicomponent interlinking among carbonvoid@silica@silicon (CVSS) nanospheres and cross-linked carboxymethyl cellulose and citric acid polymer binder (c-CMC-CA). Due to the additional protection from the silica layer, CVSS is superior to the carbon@void@silicon (CVS) electrode in terms of long-term cyclability. The as-prepared all-integrated CVSS electrode exhibits high mechanical strength, which can be ascribed to the high adhesivity and ductility of c-CMC-CA binder and the strong binding energy between CVSS and c-CMC-CA, as calculated based on density functional theory (DFT). This electrode exhibits a high reversible capacity of 1640 mA h g-1 after 100 cycles at a current density of 1 A g-1 , high rate performance, and long-term cycling stability with 84.6% capacity retention after 1000 cycles at 5 A g-1