Electrospun poly(styrene-block-dimethylsiloxane) block copolymer fibers exhibiting superhydrophobicity
Block copolymer poly(styrene-b-dimethylsiloxane) fibers with submicrometer diameters in the range 150-400 nm were produced by electrospinning from solution in tetrahydrofuran and dimethylformamide. Contact angle measurements indicate that the nonwoven fibrous mats are superhydrophobic, with a contac...