Deshielding Anions Enable Solvation Chemistry Control of LiPF6-Based Electrolyte toward Low-Temperature Lithium-Ion Batteries

© 2024 Wiley‐VCH GmbH.

Bibliographische Detailangaben
Veröffentlicht in:Advanced materials (Deerfield Beach, Fla.). - 1998. - 36(2024), 16 vom: 01. Apr., Seite e2311327
1. Verfasser: Yuan, Song (VerfasserIn)
Weitere Verfasser: Cao, Shengkai, Chen, Xi, Wei, Jiaqi, Lv, Zhisheng, Xia, Huarong, Li, Jiaofu, Zhang, Hang, Liu, Lin, Tian, Changhao, Chen, Lixun, Zhang, Wei, Xing, Zhenxiang, Li, Haicheng, Li, Shuzhou, Zhu, Qiang, Feng, Xue, Chen, Xiaodong
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2024
Zugriff auf das übergeordnete Werk:Advanced materials (Deerfield Beach, Fla.)
Schlagworte:Journal Article LiPF6‐based electrolyte deshielding anions lithium‐ion batteries low temperature solvation design
LEADER 01000caa a22002652 4500
001 NLM367120569
003 DE-627
005 20240418232450.0
007 cr uuu---uuuuu
008 240115s2024 xx |||||o 00| ||eng c
024 7 |a 10.1002/adma.202311327  |2 doi 
028 5 2 |a pubmed24n1379.xml 
035 |a (DE-627)NLM367120569 
035 |a (NLM)38221508 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Yuan, Song  |e verfasserin  |4 aut 
245 1 0 |a Deshielding Anions Enable Solvation Chemistry Control of LiPF6-Based Electrolyte toward Low-Temperature Lithium-Ion Batteries 
264 1 |c 2024 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Revised 18.04.2024 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a © 2024 Wiley‐VCH GmbH. 
520 |a Severe capacity decay under subzero temperatures remains a significant challenge for lithium-ion batteries (LIBs) due to the sluggish interfacial kinetics. Current efforts to mitigate this deteriorating interfacial behavior rely on high-solubility lithium salts (e.g., Lithium bis(trifluoromethanesulfonyl)imide (LiTFSI), Lithium bis(fluorosulfonyl)imide (LiFSI))-based electrolytes to construct anion participated solvation structures. However, such electrolytes bring issues of corrosion on the current collector and increased costs. Herein, the most commonly used Lithium hexafluorophosphate (LiPF6) instead, to establish a peculiar solvation structure with a high ratio of ion pairs and aggregates by introducing a deshielding NO3 - additive for low-temperature LIBs is utilized. The deshielding anion significantly reduces the energy barrier for interfacial behavior at low temperatures. Benefiting from this, the graphite (Gr) anode retains a high capacity of ≈72.3% at -20 °C, which is far superior to the 32.3% and 19.4% capacity retention of counterpart electrolytes. Moreover, the LiCoO2/Gr full cell exhibits a stable cycling performance of 100 cycles at -20 °C due to the inhibited lithium plating. This work heralds a new paradigm in LiPF6-based electrolyte design for LIBs operating at subzero temperatures 
650 4 |a Journal Article 
650 4 |a LiPF6‐based electrolyte 
650 4 |a deshielding anions 
650 4 |a lithium‐ion batteries 
650 4 |a low temperature 
650 4 |a solvation design 
700 1 |a Cao, Shengkai  |e verfasserin  |4 aut 
700 1 |a Chen, Xi  |e verfasserin  |4 aut 
700 1 |a Wei, Jiaqi  |e verfasserin  |4 aut 
700 1 |a Lv, Zhisheng  |e verfasserin  |4 aut 
700 1 |a Xia, Huarong  |e verfasserin  |4 aut 
700 1 |a Li, Jiaofu  |e verfasserin  |4 aut 
700 1 |a Zhang, Hang  |e verfasserin  |4 aut 
700 1 |a Liu, Lin  |e verfasserin  |4 aut 
700 1 |a Tian, Changhao  |e verfasserin  |4 aut 
700 1 |a Chen, Lixun  |e verfasserin  |4 aut 
700 1 |a Zhang, Wei  |e verfasserin  |4 aut 
700 1 |a Xing, Zhenxiang  |e verfasserin  |4 aut 
700 1 |a Li, Haicheng  |e verfasserin  |4 aut 
700 1 |a Li, Shuzhou  |e verfasserin  |4 aut 
700 1 |a Zhu, Qiang  |e verfasserin  |4 aut 
700 1 |a Feng, Xue  |e verfasserin  |4 aut 
700 1 |a Chen, Xiaodong  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Advanced materials (Deerfield Beach, Fla.)  |d 1998  |g 36(2024), 16 vom: 01. Apr., Seite e2311327  |w (DE-627)NLM098206397  |x 1521-4095  |7 nnns 
773 1 8 |g volume:36  |g year:2024  |g number:16  |g day:01  |g month:04  |g pages:e2311327 
856 4 0 |u http://dx.doi.org/10.1002/adma.202311327  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_350 
951 |a AR 
952 |d 36  |j 2024  |e 16  |b 01  |c 04  |h e2311327