Spontaneous Interface Healing by a Dynamic Liquid-Crystal Transition for High-Performance Perovskite Solar Cells

© 2022 Wiley-VCH GmbH.

Bibliographische Detailangaben
Veröffentlicht in:Advanced materials (Deerfield Beach, Fla.). - 1998. - 34(2022), 49 vom: 28. Dez., Seite e2207362
1. Verfasser: Du, Xinyi (VerfasserIn)
Weitere Verfasser: Zhang, Lu, Chen, Ran, You, Jiaxue, Ma, Yabin, Wang, Jungang, Wu, Yin, Liu, Baibai, Zhao, Kui, Chen, Jiangzhao, Chen, Xinbing, An, Zhongwei, Liu, Shengzhong Frank
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2022
Zugriff auf das übergeordnete Werk:Advanced materials (Deerfield Beach, Fla.)
Schlagworte:Journal Article crystallization retardation dynamic liquid-crystal transitions high efficiency and stability interfacial healing perovskite solar cells
LEADER 01000naa a22002652 4500
001 NLM347836313
003 DE-627
005 20231226034758.0
007 cr uuu---uuuuu
008 231226s2022 xx |||||o 00| ||eng c
024 7 |a 10.1002/adma.202207362  |2 doi 
028 5 2 |a pubmed24n1159.xml 
035 |a (DE-627)NLM347836313 
035 |a (NLM)36268995 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Du, Xinyi  |e verfasserin  |4 aut 
245 1 0 |a Spontaneous Interface Healing by a Dynamic Liquid-Crystal Transition for High-Performance Perovskite Solar Cells 
264 1 |c 2022 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Completed 09.12.2022 
500 |a Date Revised 09.12.2022 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a © 2022 Wiley-VCH GmbH. 
520 |a Low-temperature solution processing of thin-film semiconductors is more cost-effective than traditional vacuum processing; however, it leads to more defects during fast bulk crystallization and residual tensile stress. Herein, a new strategy of dynamic liquid-crystal transition (DLCT) is developed to solve these problems in one step. The design principle is used to suggest that the DLCT molecule should firstly interact with the perovskite grains in the bulk and meanwhile go through a dynamic transition to spontaneously heal the interface. A thermotropic LC molecule (CBO6SS6OCB) is then designed to demonstrate the strategy. The LC interacting with perovskite colloid forms an intermediate adduct to retard the crystallization. The annealing processes stimulate the concentrated LC solid, causing it to flow to the electron transport layer to release the residual stress to attain improved electron extraction. Consequently, the device efficiency is increased to 24.38%, where its VOC of 1.184 V is among the best for the formamidine-based perovskite solar cells. Furthermore, the ambient stability (93.0% of initial efficiency after 2000 h of aging) and light stability (96.3% of initial efficiency after 500 h of aging) are much improved. This work conceives a new engineering of additive phase transition for high-performance perovskite solar cells 
650 4 |a Journal Article 
650 4 |a crystallization retardation 
650 4 |a dynamic liquid-crystal transitions 
650 4 |a high efficiency and stability 
650 4 |a interfacial healing 
650 4 |a perovskite solar cells 
700 1 |a Zhang, Lu  |e verfasserin  |4 aut 
700 1 |a Chen, Ran  |e verfasserin  |4 aut 
700 1 |a You, Jiaxue  |e verfasserin  |4 aut 
700 1 |a Ma, Yabin  |e verfasserin  |4 aut 
700 1 |a Wang, Jungang  |e verfasserin  |4 aut 
700 1 |a Wu, Yin  |e verfasserin  |4 aut 
700 1 |a Liu, Baibai  |e verfasserin  |4 aut 
700 1 |a Zhao, Kui  |e verfasserin  |4 aut 
700 1 |a Chen, Jiangzhao  |e verfasserin  |4 aut 
700 1 |a Chen, Xinbing  |e verfasserin  |4 aut 
700 1 |a An, Zhongwei  |e verfasserin  |4 aut 
700 1 |a Liu, Shengzhong Frank  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Advanced materials (Deerfield Beach, Fla.)  |d 1998  |g 34(2022), 49 vom: 28. Dez., Seite e2207362  |w (DE-627)NLM098206397  |x 1521-4095  |7 nnns 
773 1 8 |g volume:34  |g year:2022  |g number:49  |g day:28  |g month:12  |g pages:e2207362 
856 4 0 |u http://dx.doi.org/10.1002/adma.202207362  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_350 
951 |a AR 
952 |d 34  |j 2022  |e 49  |b 28  |c 12  |h e2207362