Guidelines for Arranging 2D Nanosheets into Neatly Tiled Monolayer Films by a Spin-Coating Process

Neat (dense and nonoverlapped) monolayer tiling of 2D nanosheets on a substrate surface is very important because we can conduct artificial lattice-engineering by repeating the tiling process in a designed sequence to tailor various hierarchical nanostructures, leading to a range of sophisticated fu...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1992. - 38(2022), 40 vom: 11. Okt., Seite 12399-12407
1. Verfasser: Sakai, Nobuyuki (VerfasserIn)
Weitere Verfasser: Sasaki, Takayoshi
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2022
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article
LEADER 01000naa a22002652 4500
001 NLM346882680
003 DE-627
005 20231226032519.0
007 cr uuu---uuuuu
008 231226s2022 xx |||||o 00| ||eng c
024 7 |a 10.1021/acs.langmuir.2c02211  |2 doi 
028 5 2 |a pubmed24n1156.xml 
035 |a (DE-627)NLM346882680 
035 |a (NLM)36172710 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Sakai, Nobuyuki  |e verfasserin  |4 aut 
245 1 0 |a Guidelines for Arranging 2D Nanosheets into Neatly Tiled Monolayer Films by a Spin-Coating Process 
264 1 |c 2022 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Revised 11.10.2022 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a Neat (dense and nonoverlapped) monolayer tiling of 2D nanosheets on a substrate surface is very important because we can conduct artificial lattice-engineering by repeating the tiling process in a designed sequence to tailor various hierarchical nanostructures, leading to a range of sophisticated functions. It is recently reported that a facile spin-coating technique realizes the neat monolayer tiling of various 2D nanosheets. Establishing universal guidelines to neatly tile 2D nanosheets on substrates of various materials and size/shape is of essential importance to fully apply this technique, but the mechanism of how the nanosheets are tiled has not been clarified yet. In the present study, we have systematically examined the nanosheet deposition process at various rotation speeds by microscopic observations and found that the neat monolayer tiling of nanosheets is attained on the solvent surface during the spin-coating, and then the monolayer film is deposited onto the substrate surface from its center toward the edges upon evaporation of the solvent. Furthermore, we have clarified how the rotation speed and the nanosheet concentration govern the deposition behaviors in terms of neat tiling, overlap, or noncoverage in a such process. On the basis of the guidelines, we can predict the optimum spin-coating conditions for attaining the neat monolayer tiling of various nanosheets over an entire surface of the substrate 
650 4 |a Journal Article 
700 1 |a Sasaki, Takayoshi  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1992  |g 38(2022), 40 vom: 11. Okt., Seite 12399-12407  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:38  |g year:2022  |g number:40  |g day:11  |g month:10  |g pages:12399-12407 
856 4 0 |u http://dx.doi.org/10.1021/acs.langmuir.2c02211  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 38  |j 2022  |e 40  |b 11  |c 10  |h 12399-12407