Elucidating the Initial Steps in α-Uranium Hydriding Using First-Principles Calculations

Hydrogen embrittlement of uranium, which arises due to the formation of a structurally weak pyrophoric hydride, poses a major safety risk in material applications. Previous experiments have shown that hydriding begins on the top or near the surface (i.e., subsurface) of α-uranium. However, the funda...