Surface Wrinkling on Polymer Films

A series of gold precursor solutions are prepared by dissolving HAuCl4 and its mixtures with K2CO3 of different contents in deionized (DI) water. Neat HAuCl4 predominately forms AuCl4- ions in an aqueous solution. In the presence of K2CO3, AuCl4- ions hydrolyze to form [AuCl4-x(OH)x]- complex ions....

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1992. - 38(2022), 12 vom: 29. März, Seite 3907-3916
1. Verfasser: Junisu, Belda Amelia (VerfasserIn)
Weitere Verfasser: Chang, Iris Ching-Ya, Lin, Chia-Chi, Sun, Ya-Sen
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2022
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article
LEADER 01000naa a22002652 4500
001 NLM338288104
003 DE-627
005 20231226000332.0
007 cr uuu---uuuuu
008 231226s2022 xx |||||o 00| ||eng c
024 7 |a 10.1021/acs.langmuir.2c00156  |2 doi 
028 5 2 |a pubmed24n1127.xml 
035 |a (DE-627)NLM338288104 
035 |a (NLM)35298168 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Junisu, Belda Amelia  |e verfasserin  |4 aut 
245 1 0 |a Surface Wrinkling on Polymer Films 
264 1 |c 2022 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Revised 29.03.2022 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a A series of gold precursor solutions are prepared by dissolving HAuCl4 and its mixtures with K2CO3 of different contents in deionized (DI) water. Neat HAuCl4 predominately forms AuCl4- ions in an aqueous solution. In the presence of K2CO3, AuCl4- ions hydrolyze to form [AuCl4-x(OH)x]- complex ions. Increasing the content of K2CO3 in a gold precursor solution increases the content of [AuCl4-x(OH)x]- complex ions and decreases the content of AuCl4- ions. Poly(4-vinyl pyridine) (P4VP) films of two different molecular weights are deposited on SiOx/Si by spin coating, by which the thicknesses are controlled by polymer weight fractions in butanol. Those P4VP films form periodic wrinkles when immersed in aqueous solutions, followed by drying. The surface wrinkling is induced by swelling pressure that overwhelms the mechanical property of the P4VP film. The periodicity and amplitude of wrinkles grown on the P4VP films strongly correlate with initial thickness, AuCl4- ion content, and residual stress 
650 4 |a Journal Article 
700 1 |a Chang, Iris Ching-Ya  |e verfasserin  |4 aut 
700 1 |a Lin, Chia-Chi  |e verfasserin  |4 aut 
700 1 |a Sun, Ya-Sen  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1992  |g 38(2022), 12 vom: 29. März, Seite 3907-3916  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:38  |g year:2022  |g number:12  |g day:29  |g month:03  |g pages:3907-3916 
856 4 0 |u http://dx.doi.org/10.1021/acs.langmuir.2c00156  |3 Volltext 