Morphology of Mixed Langmuir and Langmuir-Schaefer Monolayers with Covered CdSe/CdS/ZnS Quantum Dots and Arachidic Acid

The process of formation of a Langmuir-Schaefer (LS) matrix based on a mixed monolayer of arachidic acid (AA) and 8 nm CdSe/CdS/ZnS quantum dots (QDs) stabilized by molecules of trioctylphosphine oxide (TOPO) was investigated. The change in the morphology, monolayer compressibility, and area per ele...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1999. - 37(2021), 48 vom: 07. Dez., Seite 14105-14113
1. Verfasser: Gorbachev, Ilya A (VerfasserIn)
Weitere Verfasser: Smirnov, Andrey V, Glukhovskoy, Evgeny G, Kolesov, Vladimir V, Ivanov, George R, Kuznetsova, Iren E
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2021
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article
LEADER 01000naa a22002652 4500
001 NLM333310810
003 DE-627
005 20231225221410.0
007 cr uuu---uuuuu
008 231225s2021 xx |||||o 00| ||eng c
024 7 |a 10.1021/acs.langmuir.1c02345  |2 doi 
028 5 2 |a pubmed24n1110.xml 
035 |a (DE-627)NLM333310810 
035 |a (NLM)34793676 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Gorbachev, Ilya A  |e verfasserin  |4 aut 
245 1 0 |a Morphology of Mixed Langmuir and Langmuir-Schaefer Monolayers with Covered CdSe/CdS/ZnS Quantum Dots and Arachidic Acid 
264 1 |c 2021 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Revised 07.12.2021 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a The process of formation of a Langmuir-Schaefer (LS) matrix based on a mixed monolayer of arachidic acid (AA) and 8 nm CdSe/CdS/ZnS quantum dots (QDs) stabilized by molecules of trioctylphosphine oxide (TOPO) was investigated. The change in the morphology, monolayer compressibility, and area per elementary cell of the created mixed monolayers, depending on the ratio of the components, was studied. It is shown that the change in the morphology of Langmuir-Blodgett (LB) monolayers begins to occur at a ratio between the number of QDs and AA molecules of 1:24. Dendrimeric structures with a thickness of the order of 30-40 nm appear in the mixed monolayer when LB film deposition was carried out above the collapse surface pressure of a Langmuir film from only TOPO-covered QDs. Information on the dependence of the morphology of such structures on the molar ratio of the components is necessary for the production of ordered 2D nanostructures containing 0D and 1D objects with quantum bonds. Such nanostructures can be used in nanoelectronic and optoelectronic devices as a sensitive sensor element. The obtained results would be relevant for any type of spherical shape nanoparticles 
650 4 |a Journal Article 
700 1 |a Smirnov, Andrey V  |e verfasserin  |4 aut 
700 1 |a Glukhovskoy, Evgeny G  |e verfasserin  |4 aut 
700 1 |a Kolesov, Vladimir V  |e verfasserin  |4 aut 
700 1 |a Ivanov, George R  |e verfasserin  |4 aut 
700 1 |a Kuznetsova, Iren E  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1999  |g 37(2021), 48 vom: 07. Dez., Seite 14105-14113  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:37  |g year:2021  |g number:48  |g day:07  |g month:12  |g pages:14105-14113 
856 4 0 |u http://dx.doi.org/10.1021/acs.langmuir.1c02345  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 37  |j 2021  |e 48  |b 07  |c 12  |h 14105-14113