Bipolar Electrochemical Anodization Route for the Fabrication of Porous Anodic Alumina with Nanopore Gradients

Porous anodic alumina (PAA) films with homogeneous nanopores are achieved by traditional anodization. Here, we present a unique anodization technique based on bipolar electrochemistry to fabricate PAA films with nanopore gradients. In an oxalic acid solution dissolved in ethylene glycol, a stable bi...

Description complète

Détails bibliographiques
Publié dans:Langmuir : the ACS journal of surfaces and colloids. - 1985. - 37(2021), 14 vom: 13. Apr., Seite 4340-4346
Auteur principal: Yang, Yan (Auteur)
Autres auteurs: Xu, Dawei, Liu, Qianqian, Wang, Qi, Yu, Huiwen, Zhu, Xufei, Song, Ye
Format: Article en ligne
Langue:English
Publié: 2021
Accès à la collection:Langmuir : the ACS journal of surfaces and colloids
Sujets:Journal Article
LEADER 01000caa a22002652c 4500
001 NLM323479634
003 DE-627
005 20250301081906.0
007 cr uuu---uuuuu
008 231225s2021 xx |||||o 00| ||eng c
024 7 |a 10.1021/acs.langmuir.1c00405  |2 doi 
028 5 2 |a pubmed25n1078.xml 
035 |a (DE-627)NLM323479634 
035 |a (NLM)33792327 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Yang, Yan  |e verfasserin  |4 aut 
245 1 0 |a Bipolar Electrochemical Anodization Route for the Fabrication of Porous Anodic Alumina with Nanopore Gradients 
264 1 |c 2021 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Revised 13.04.2021 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a Porous anodic alumina (PAA) films with homogeneous nanopores are achieved by traditional anodization. Here, we present a unique anodization technique based on bipolar electrochemistry to fabricate PAA films with nanopore gradients. In an oxalic acid solution dissolved in ethylene glycol, a stable bipolar anodization process is realized. The PAA film prepared at 280 V exhibits a continuous change in interpore distance from ∼171 to ∼83 nm over a range of only 5 mm on the aluminum sheet. Higher driving voltages lead to larger interpore distances and steeper nanopore gradients. Further, no direct electrical connection is required for this bipolar anodization 
650 4 |a Journal Article 
700 1 |a Xu, Dawei  |e verfasserin  |4 aut 
700 1 |a Liu, Qianqian  |e verfasserin  |4 aut 
700 1 |a Wang, Qi  |e verfasserin  |4 aut 
700 1 |a Yu, Huiwen  |e verfasserin  |4 aut 
700 1 |a Zhu, Xufei  |e verfasserin  |4 aut 
700 1 |a Song, Ye  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1985  |g 37(2021), 14 vom: 13. Apr., Seite 4340-4346  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnas 
773 1 8 |g volume:37  |g year:2021  |g number:14  |g day:13  |g month:04  |g pages:4340-4346 
856 4 0 |u http://dx.doi.org/10.1021/acs.langmuir.1c00405  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 37  |j 2021  |e 14  |b 13  |c 04  |h 4340-4346