Fabrication and characterization of polysulfone reinforced hollow fibre membrane
In this study, reinforced hollow fibre membranes were fabricated using different molecular weights of polyvinylidene prolidone (PVP Mw: 10, 40 and 360 kDa) and different take-up speeds (1, 2, 2.6 and 3.5 m/min). Prepared reinforced hollow fibre membranes were characterized in terms of permeability;...
Description complète
Détails bibliographiques
Publié dans: | Environmental technology. - 1993. - 42(2021), 17 vom: 01. Juli, Seite 2690-2699
|
Auteur principal: |
Turken, Turker
(Auteur) |
Autres auteurs: |
Sengur-Tasdemir, Reyhan,
Urper-Bayram, Gulsum Melike,
Gunes, Oguz,
Ates-Genceli, Esra,
Tarabara, Volodymyr V,
Koyuncu, Ismail |
Format: | Article en ligne
|
Langue: | English |
Publié: |
2021
|
Accès à la collection: | Environmental technology
|
Sujets: | Journal Article
Reinforced
hollow fibre
membrane fabrication
polyvinylidene prolidone
Membranes, Artificial
Polymers
Sulfones
polysulfone P 1700
25135-51-7 |