Effect of Ethanethiolate Spacer on Morphology and Optical Responses of Ag Nanoparticle Array-Single Layer Graphene Hybrid Systems

Single layer graphene (SLG) and two-dimensional (2-D) plasmonic Ag nanoparticle arrays assembled by chemisorption of ethanethiol (ET) molecules (AgNPs-ET) were employed as components of two types of hybrid systems designed for surface-enhanced Raman scattering (SERS) spectral probing of SLG localize...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1992. - 33(2017), 50 vom: 19. Dez., Seite 14414-14424
1. Verfasser: Sutrová, Veronika (VerfasserIn)
Weitere Verfasser: Šloufová, Ivana, Melníková, Zuzana, Kalbáč, Martin, Pavlova, Ewa, Vlčková, Blanka
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2017
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article Research Support, Non-U.S. Gov't
LEADER 01000naa a22002652 4500
001 NLM27838434X
003 DE-627
005 20231225020441.0
007 cr uuu---uuuuu
008 231225s2017 xx |||||o 00| ||eng c
024 7 |a 10.1021/acs.langmuir.7b03462  |2 doi 
028 5 2 |a pubmed24n0927.xml 
035 |a (DE-627)NLM27838434X 
035 |a (NLM)29172530 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Sutrová, Veronika  |e verfasserin  |4 aut 
245 1 0 |a Effect of Ethanethiolate Spacer on Morphology and Optical Responses of Ag Nanoparticle Array-Single Layer Graphene Hybrid Systems 
264 1 |c 2017 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Completed 06.08.2018 
500 |a Date Revised 06.08.2018 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a Single layer graphene (SLG) and two-dimensional (2-D) plasmonic Ag nanoparticle arrays assembled by chemisorption of ethanethiol (ET) molecules (AgNPs-ET) were employed as components of two types of hybrid systems designed for surface-enhanced Raman scattering (SERS) spectral probing of SLG localized in the vicinity of plasmonic NPs. Both hybrids were characterized by optical microscopy, transmission electron microscopy (TEM), surface plasmon extinction (SPE), and SERS microRaman spectral measurements at four excitation wavelengths spanning the 445-780 nm range. SERS spectral probing of the glass/SLG/AgNPs-ET hybrid prepared by overdeposition of SLG on glass by the array of ET-modified Ag NPs has shown that the chemisorbed ET acts as an efficient molecular spacer between SLG and Ag NPs surface which, in turn, enabled to obtain SERS spectra of SLG unperturbed by doping or strain. TEM imaging and SERS spectral probing of the second hybrid prepared by overdeposition of AgNPs-ET array on glass by SLG revealed removal of the adsorbed ET molecules and annealing of Ag NPs during the SLG deposition. The characteristics of the resulting glass/AgNPs/SLG hybrid system, namely (i) broad distribution of the annealed Ag NPs sizes and shapes, (ii) SPE curve covering the overall visible spectral region, (iii) absence of the ET spectral bands in SERS spectra, and (iv) fairly uniform SERS enhancement of the G and 2D mode of SLG in the 532-780 nm range in the straight sample geometry indicate that this hybrid can provide a suitable platform for investigation of the excitation wavelength dependence of combined SERS/GERS (graphene-enhanced Raman scattering) enhancement experienced by various molecular species brought into contact with SLG in this hybrid. Finally, weak optical effects attributed to increased reflectivity of SLG in the near field of Ag NPs arrays have been observed in the excitation wavelength dependence of the SERS spectra of both types of hybrid systems 
650 4 |a Journal Article 
650 4 |a Research Support, Non-U.S. Gov't 
700 1 |a Šloufová, Ivana  |e verfasserin  |4 aut 
700 1 |a Melníková, Zuzana  |e verfasserin  |4 aut 
700 1 |a Kalbáč, Martin  |e verfasserin  |4 aut 
700 1 |a Pavlova, Ewa  |e verfasserin  |4 aut 
700 1 |a Vlčková, Blanka  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1992  |g 33(2017), 50 vom: 19. Dez., Seite 14414-14424  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:33  |g year:2017  |g number:50  |g day:19  |g month:12  |g pages:14414-14424 
856 4 0 |u http://dx.doi.org/10.1021/acs.langmuir.7b03462  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 33  |j 2017  |e 50  |b 19  |c 12  |h 14414-14424