Effects of waste glass and waste foundry sand additions on reclaimed tiles containing sewage sludge ash

Applying sewage sludge ash (SSA) to produce reclaimed tiles is a promising recycling technology in resolving the increasing sludge wastes from wastewater treatment. However, performance of such reclaimed tiles is inferior to that of original ceramic tiles. Many researchers have therefore tried addin...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Environmental technology. - 1998. - 38(2017), 13-14 vom: 28. Juli, Seite 1679-1688
1. Verfasser: Lin, Deng-Fong (VerfasserIn)
Weitere Verfasser: Luo, Huan-Lin, Lin, Kuo-Liang, Liu, Zhe-Kun
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2017
Zugriff auf das übergeordnete Werk:Environmental technology
Schlagworte:Journal Article Reclaimed tile clay sewage sludge ash waste foundry sand waste glass Aluminum Silicates Industrial Waste Metals Sewage mehr... Water Pollutants, Chemical Clay T1FAD4SS2M
LEADER 01000caa a22002652 4500
001 NLM269698345
003 DE-627
005 20250221082307.0
007 cr uuu---uuuuu
008 231224s2017 xx |||||o 00| ||eng c
024 7 |a 10.1080/09593330.2017.1296891  |2 doi 
028 5 2 |a pubmed25n0898.xml 
035 |a (DE-627)NLM269698345 
035 |a (NLM)28278768 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Lin, Deng-Fong  |e verfasserin  |4 aut 
245 1 0 |a Effects of waste glass and waste foundry sand additions on reclaimed tiles containing sewage sludge ash 
264 1 |c 2017 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Completed 11.10.2017 
500 |a Date Revised 02.12.2018 
500 |a published: Print-Electronic 
500 |a Citation Status MEDLINE 
520 |a Applying sewage sludge ash (SSA) to produce reclaimed tiles is a promising recycling technology in resolving the increasing sludge wastes from wastewater treatment. However, performance of such reclaimed tiles is inferior to that of original ceramic tiles. Many researchers have therefore tried adding various industrial by-products to improve reclaimed tile properties. In this study, multiple materials including waste glass and waste foundry sand (WFS) were added in an attempt to improve physical and mechanical properties of reclaimed tiles with SSA. Samples with various combinations of clay, WFS, waste glass and SSA were made with three kiln temperatures of 1000°C, 1050°C, and 1100°C. A series of tests on the samples were next conducted. Test results showed that waste glass had positive effects on bending strength, water absorption and weight loss on ignition, while WFS contributed the most in reducing shrinkage, but could decrease the tile bending strength when large amount was added at a high kiln temperature. This study suggested that a combination of WFS from 10% to 15%, waste glass from 15% to 20%, SSA at 10% at a kiln temperature between 1000°C and 1050°C could result in quality reclaimed tiles with a balanced performance 
650 4 |a Journal Article 
650 4 |a Reclaimed tile 
650 4 |a clay 
650 4 |a sewage sludge ash 
650 4 |a waste foundry sand 
650 4 |a waste glass 
650 7 |a Aluminum Silicates  |2 NLM 
650 7 |a Industrial Waste  |2 NLM 
650 7 |a Metals  |2 NLM 
650 7 |a Sewage  |2 NLM 
650 7 |a Water Pollutants, Chemical  |2 NLM 
650 7 |a Clay  |2 NLM 
650 7 |a T1FAD4SS2M  |2 NLM 
700 1 |a Luo, Huan-Lin  |e verfasserin  |4 aut 
700 1 |a Lin, Kuo-Liang  |e verfasserin  |4 aut 
700 1 |a Liu, Zhe-Kun  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Environmental technology  |d 1998  |g 38(2017), 13-14 vom: 28. Juli, Seite 1679-1688  |w (DE-627)NLM098202545  |x 1479-487X  |7 nnns 
773 1 8 |g volume:38  |g year:2017  |g number:13-14  |g day:28  |g month:07  |g pages:1679-1688 
856 4 0 |u http://dx.doi.org/10.1080/09593330.2017.1296891  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_350 
951 |a AR 
952 |d 38  |j 2017  |e 13-14  |b 28  |c 07  |h 1679-1688