Evolution of the PVP-Pd Surface Interaction in Nanoparticles through the Case Study of Formic Acid Decomposition

Palladium nanoparticles (Pd NPs) were synthesized by the reduction-by-solvent method using polyvinylpirrolidone (PVP) as capping agent. The nonstatic interaction between PVP and the metallic surface may change the properties of the NPs due to the different possible interactions, through either the O...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1999. - 32(2016), 46 vom: 22. Nov., Seite 12110-12118
1. Verfasser: García-Aguilar, Jaime (VerfasserIn)
Weitere Verfasser: Navlani-García, Miriam, Berenguer-Murcia, Ángel, Mori, Kohsuke, Kuwahara, Yasutaka, Yamashita, Hiromi, Cazorla-Amorós, Diego
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2016
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article Research Support, Non-U.S. Gov't
LEADER 01000naa a22002652 4500
001 NLM265707080
003 DE-627
005 20231224212856.0
007 cr uuu---uuuuu
008 231224s2016 xx |||||o 00| ||eng c
028 5 2 |a pubmed24n0885.xml 
035 |a (DE-627)NLM265707080 
035 |a (NLM)27788005 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a García-Aguilar, Jaime  |e verfasserin  |4 aut 
245 1 0 |a Evolution of the PVP-Pd Surface Interaction in Nanoparticles through the Case Study of Formic Acid Decomposition 
264 1 |c 2016 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Completed 18.07.2018 
500 |a Date Revised 18.07.2018 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a Palladium nanoparticles (Pd NPs) were synthesized by the reduction-by-solvent method using polyvinylpirrolidone (PVP) as capping agent. The nonstatic interaction between PVP and the metallic surface may change the properties of the NPs due to the different possible interactions, through either the O or N atoms of the PVP. In order to analyze these effects and their repercussions in their catalytic performance, Pd NPs with various PVP/Pd molar ratios (1, 10, and 20) were prepared, deposited on silica, and tested in the formic acid decomposition reaction. The catalytic tests were conducted using catalysts prepared by loading NPs with three different time lapses between their purification and their deposition on the silica support (1 day, 1 month, and 6 months). CO adsorption, FTIR spectroscopy, XPS, and TEM characterization were used to determine the accessibility of the Pd NPs surface sites, the electronic state of Pd, and the average NPs size, respectively. The H2 production from the formic acid decomposition reaction has a strong dependence on the Pd surface features, which in turn are related to the NPs aging time due to the progressive removal of the PVP 
650 4 |a Journal Article 
650 4 |a Research Support, Non-U.S. Gov't 
700 1 |a Navlani-García, Miriam  |e verfasserin  |4 aut 
700 1 |a Berenguer-Murcia, Ángel  |e verfasserin  |4 aut 
700 1 |a Mori, Kohsuke  |e verfasserin  |4 aut 
700 1 |a Kuwahara, Yasutaka  |e verfasserin  |4 aut 
700 1 |a Yamashita, Hiromi  |e verfasserin  |4 aut 
700 1 |a Cazorla-Amorós, Diego  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1999  |g 32(2016), 46 vom: 22. Nov., Seite 12110-12118  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:32  |g year:2016  |g number:46  |g day:22  |g month:11  |g pages:12110-12118 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 32  |j 2016  |e 46  |b 22  |c 11  |h 12110-12118