Debonding mechanisms of soft materials at short contact times

A carefully controlled, custom-built adhesion testing device was developed which allows a precise, short dwell time on the order of milliseconds to be applied during a contact adhesion experiment. The dwell time dependence of the adhesive strength of crosslinked poly(dimethylsiloxane) (PDMS) in cont...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1992. - 30(2014), 35 vom: 09. Sept., Seite 10626-36
1. Verfasser: Davis, Chelsea S (VerfasserIn)
Weitere Verfasser: Lemoine, Florian, Darnige, Thierry, Martina, David, Creton, Costantino, Lindner, Anke
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2014
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article
LEADER 01000naa a22002652 4500
001 NLM241018889
003 DE-627
005 20231224123336.0
007 cr uuu---uuuuu
008 231224s2014 xx |||||o 00| ||eng c
024 7 |a 10.1021/la5023592  |2 doi 
028 5 2 |a pubmed24n0803.xml 
035 |a (DE-627)NLM241018889 
035 |a (NLM)25127556 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Davis, Chelsea S  |e verfasserin  |4 aut 
245 1 0 |a Debonding mechanisms of soft materials at short contact times 
264 1 |c 2014 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Completed 15.05.2015 
500 |a Date Revised 09.09.2014 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a A carefully controlled, custom-built adhesion testing device was developed which allows a precise, short dwell time on the order of milliseconds to be applied during a contact adhesion experiment. The dwell time dependence of the adhesive strength of crosslinked poly(dimethylsiloxane) (PDMS) in contact with glass and uncrosslinked styrene butadiene rubber (SBR) in contact with glass and with itself was tested with a spherical probe in a confined Johnson-Kendall-Roberts (JKR) geometry. Analysis of the contact images revealed several unique separation mechanisms which are dependent on dwell time and interfacial properties. PDMS-glass interfaces show essentially no dependence of adhesion on the dwell time while the adhesive strength and separation mechanisms of SBR interfaces are shown to vary drastically for dwell times ranging from 40 to 10,000 ms. This influence of dwell time is particularly pronounced for polymer-polymer (SBR-SBR) interfaces. Observations of cavitation due to trapped air pockets in the center of the contact at very short contact times illustrate a transition between a defect-controlled debonding and an interface-controlled debonding which has not been previously reported 
650 4 |a Journal Article 
700 1 |a Lemoine, Florian  |e verfasserin  |4 aut 
700 1 |a Darnige, Thierry  |e verfasserin  |4 aut 
700 1 |a Martina, David  |e verfasserin  |4 aut 
700 1 |a Creton, Costantino  |e verfasserin  |4 aut 
700 1 |a Lindner, Anke  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1992  |g 30(2014), 35 vom: 09. Sept., Seite 10626-36  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:30  |g year:2014  |g number:35  |g day:09  |g month:09  |g pages:10626-36 
856 4 0 |u http://dx.doi.org/10.1021/la5023592  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 30  |j 2014  |e 35  |b 09  |c 09  |h 10626-36