This work features the controllability of surface-initiated atom transfer radical polymerization (SI-ATRP) of methyl methacrylate, initiated by a multilayered 2-bromoisobutyryl moiety formed via diazonium chemistry. The thickness as a function of polymerization time has been studied by varying diffe...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1992. - 27(2011), 3 vom: 01. Feb., Seite 1070-8
1. Verfasser: Iruthayaraj, Joseph (VerfasserIn)
Weitere Verfasser: Chernyy, Sergey, Lillethorup, Mie, Ceccato, Marcel, Røn, Troels, Hinge, Mogens, Kingshott, Peter, Besenbacher, Flemming, Pedersen, Steen Uttrup, Daasbjerg, Kim
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2011
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article
LEADER 01000naa a22002652 4500
001 NLM204504945
003 DE-627
005 20231223232145.0
007 cr uuu---uuuuu
008 231223s2011 xx |||||o 00| ||eng c
024 7 |a 10.1021/la104125n  |2 doi 
028 5 2 |a pubmed24n0682.xml 
035 |a (DE-627)NLM204504945 
035 |a (NLM)21174427 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Iruthayaraj, Joseph  |e verfasserin  |4 aut 
245 1 0 |a On surface-initiated atom transfer radical polymerization using diazonium chemistry to introduce the initiator layer 
264 1 |c 2011 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Completed 02.05.2011 
500 |a Date Revised 25.01.2011 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a This work features the controllability of surface-initiated atom transfer radical polymerization (SI-ATRP) of methyl methacrylate, initiated by a multilayered 2-bromoisobutyryl moiety formed via diazonium chemistry. The thickness as a function of polymerization time has been studied by varying different parameters such as the bromine content of the initiator layer, polarity of reaction medium, ligand type (L), and the ratio of activator (Cu(I)) to deactivator (Cu(II)) in order to ascertain the controllability of the SI-ATRP process. The variation of thickness versus surface concentration of bromine shows a gradual transition from mushroom to brush-type conformation of the surface anchored chains in both polar and nonpolar reaction medium. Interestingly, it is revealed that very thick polymer brushes, on the order of 1 μm, can be obtained at high bromine content of the initiator layer in toluene. The initial polymerization rate and the overall final thickness are higher in the case of nonpolar solvent (toluene) compared to polar medium (acetonitrile or N,N-dimethylformamide). The ligand affects the initial rate of polymerization, which correlates with the redox potentials of the pertinent Cu(II)/Cu(I) complexes (L = Me(6)TREN, PMDETA, and BIPY). It is also observed that the ability of polymer brushes to reinitiate depends on the initial thickness and the solvent used for generating it 
650 4 |a Journal Article 
700 1 |a Chernyy, Sergey  |e verfasserin  |4 aut 
700 1 |a Lillethorup, Mie  |e verfasserin  |4 aut 
700 1 |a Ceccato, Marcel  |e verfasserin  |4 aut 
700 1 |a Røn, Troels  |e verfasserin  |4 aut 
700 1 |a Hinge, Mogens  |e verfasserin  |4 aut 
700 1 |a Kingshott, Peter  |e verfasserin  |4 aut 
700 1 |a Besenbacher, Flemming  |e verfasserin  |4 aut 
700 1 |a Pedersen, Steen Uttrup  |e verfasserin  |4 aut 
700 1 |a Daasbjerg, Kim  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1992  |g 27(2011), 3 vom: 01. Feb., Seite 1070-8  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:27  |g year:2011  |g number:3  |g day:01  |g month:02  |g pages:1070-8 
856 4 0 |u http://dx.doi.org/10.1021/la104125n  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 27  |j 2011  |e 3  |b 01  |c 02  |h 1070-8