Thickness and elastic modulus of plasma treated PDMS silica-like surface layer

The adhesion of poly(dimethylsiloxane) (PDMS) rubber is largely improved by oxygen plasma surface treatment. The thickness of the silica-like surface layer is characterized by performing transmission electron microscopy imagery on microtome slices of welded plasma treated surfaces. The specific doub...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1991. - 26(2010), 5 vom: 02. März, Seite 3372-5
1. Verfasser: Béfahy, Stéphane (VerfasserIn)
Weitere Verfasser: Lipnik, Pascale, Pardoen, Thomas, Nascimento, Cristiane, Patris, Benjamin, Bertrand, Patrick, Yunus, Sami
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2010
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article Research Support, Non-U.S. Gov't Dimethylpolysiloxanes baysilon 63148-62-9 Silicon Dioxide 7631-86-9
LEADER 01000caa a22002652 4500
001 NLM193146703
003 DE-627
005 20250211013249.0
007 cr uuu---uuuuu
008 231223s2010 xx |||||o 00| ||eng c
024 7 |a 10.1021/la903154y  |2 doi 
028 5 2 |a pubmed25n0644.xml 
035 |a (DE-627)NLM193146703 
035 |a (NLM)19947617 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Béfahy, Stéphane  |e verfasserin  |4 aut 
245 1 0 |a Thickness and elastic modulus of plasma treated PDMS silica-like surface layer 
264 1 |c 2010 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Completed 28.05.2010 
500 |a Date Revised 23.02.2010 
500 |a published: Print 
500 |a Citation Status MEDLINE 
520 |a The adhesion of poly(dimethylsiloxane) (PDMS) rubber is largely improved by oxygen plasma surface treatment. The thickness of the silica-like surface layer is characterized by performing transmission electron microscopy imagery on microtome slices of welded plasma treated surfaces. The specific double layer contrast can be considered as equal to twice the thickness of the silica-like layer. The thickness measurements combined with strain-induced elastic buckling instability analysis gives an estimate of the elastic modulus of the silica-like layer equal to 1.5 GPa 
650 4 |a Journal Article 
650 4 |a Research Support, Non-U.S. Gov't 
650 7 |a Dimethylpolysiloxanes  |2 NLM 
650 7 |a baysilon  |2 NLM 
650 7 |a 63148-62-9  |2 NLM 
650 7 |a Silicon Dioxide  |2 NLM 
650 7 |a 7631-86-9  |2 NLM 
700 1 |a Lipnik, Pascale  |e verfasserin  |4 aut 
700 1 |a Pardoen, Thomas  |e verfasserin  |4 aut 
700 1 |a Nascimento, Cristiane  |e verfasserin  |4 aut 
700 1 |a Patris, Benjamin  |e verfasserin  |4 aut 
700 1 |a Bertrand, Patrick  |e verfasserin  |4 aut 
700 1 |a Yunus, Sami  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1991  |g 26(2010), 5 vom: 02. März, Seite 3372-5  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:26  |g year:2010  |g number:5  |g day:02  |g month:03  |g pages:3372-5 
856 4 0 |u http://dx.doi.org/10.1021/la903154y  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 26  |j 2010  |e 5  |b 02  |c 03  |h 3372-5