In situ observation of gamma-Fe2O3 nanoparticle adsorption under different monolayers at the air/water interface

We studied the adsorption of gamma-Fe 2O 3 nanoparticles from an aqueous solution under different charged Langmuir monolayers (stearic acid, stearyl alcohol, and stearyl amine). The aqueous subphase was composed of a colloidal suspension of gamma-Fe 2O 3 nanoparticles. The average hydrodynamic diame...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1992. - 24(2008), 22 vom: 18. Nov., Seite 12958-62
1. Verfasser: Degen, Patrick (VerfasserIn)
Weitere Verfasser: Paulus, Michael, Maas, Michael, Kahner, Rainer, Schmacke, Saskia, Struth, Bernd, Tolan, Metin, Rehage, Heinz
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2008
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article
LEADER 01000naa a22002652 4500
001 NLM18298012X
003 DE-627
005 20231223163807.0
007 cr uuu---uuuuu
008 231223s2008 xx |||||o 00| ||eng c
024 7 |a 10.1021/la802394a  |2 doi 
028 5 2 |a pubmed24n0610.xml 
035 |a (DE-627)NLM18298012X 
035 |a (NLM)18850729 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Degen, Patrick  |e verfasserin  |4 aut 
245 1 0 |a In situ observation of gamma-Fe2O3 nanoparticle adsorption under different monolayers at the air/water interface 
264 1 |c 2008 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Completed 09.01.2009 
500 |a Date Revised 13.11.2008 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a We studied the adsorption of gamma-Fe 2O 3 nanoparticles from an aqueous solution under different charged Langmuir monolayers (stearic acid, stearyl alcohol, and stearyl amine). The aqueous subphase was composed of a colloidal suspension of gamma-Fe 2O 3 nanoparticles. The average hydrodynamic diameter of the nanoparticles measured by dynamic light scattering measurements was 16 nm. The observed zeta potential of +40 mV (at pH 4) results in a long-term stability of the colloidal dispersion. The behavior of the different monolayer/nanoparticle composites were studied with surface pressure/area (pi/ A) isotherms. The adsorption of the nanoparticles under the different monolayers induced an expansion of the monolayers. These phenomena depended on the charge of the monolayers. After the Langmuir/Blodgett transfer on glass substrates, the nanoparticle/monolayer composite films were studied by means of UV-vis spectroscopy. The spectra pointed to increasing adsorption of the nanoparticles with increasing electronegativity of the monolayers. On the basis of these results, we studied the in situ adsorption of nanoparticles under the different monolayers by X-ray reflectivity measurements. Electron density profiles of the liquid/gas interfaces were obtained from the X-ray reflectivity data. The results gave clear evidence for the presence of electrostatic interaction between the differently charged monolayers and the positively charged nanoparticles. While the adsorption process was favored by the negatively charged stearic acid monolayer, the positively charged layer of stearyl amine prevented the formation of ultrathin nanoparticle layers 
650 4 |a Journal Article 
700 1 |a Paulus, Michael  |e verfasserin  |4 aut 
700 1 |a Maas, Michael  |e verfasserin  |4 aut 
700 1 |a Kahner, Rainer  |e verfasserin  |4 aut 
700 1 |a Schmacke, Saskia  |e verfasserin  |4 aut 
700 1 |a Struth, Bernd  |e verfasserin  |4 aut 
700 1 |a Tolan, Metin  |e verfasserin  |4 aut 
700 1 |a Rehage, Heinz  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1992  |g 24(2008), 22 vom: 18. Nov., Seite 12958-62  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:24  |g year:2008  |g number:22  |g day:18  |g month:11  |g pages:12958-62 
856 4 0 |u http://dx.doi.org/10.1021/la802394a  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 24  |j 2008  |e 22  |b 18  |c 11  |h 12958-62