Isotope tracer study of hydrogen spillover on carbon-based adsorbents for hydrogen storage

A composite material comprising platinum nanoparticles supported on molecular sieve templated carbon was synthesized and found to adsorb 1.35 wt % hydrogen at 298 K and 100 atm. The isosteric heat of adsorption for the material at low coverage was approximately 14 kJ/mol, and it approached a value o...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1992. - 24(2008), 12 vom: 17. Juni, Seite 6159-65
1. Verfasser: Lachawiec, Anthony J Jr (VerfasserIn)
Weitere Verfasser: Yang, Ralph T
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 2008
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article
LEADER 01000naa a22002652 4500
001 NLM17948432X
003 DE-627
005 20231223153849.0
007 cr uuu---uuuuu
008 231223s2008 xx |||||o 00| ||eng c
024 7 |a 10.1021/la800371j  |2 doi 
028 5 2 |a pubmed24n0598.xml 
035 |a (DE-627)NLM17948432X 
035 |a (NLM)18470999 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Lachawiec, Anthony J  |c Jr  |e verfasserin  |4 aut 
245 1 0 |a Isotope tracer study of hydrogen spillover on carbon-based adsorbents for hydrogen storage 
264 1 |c 2008 
336 |a Text  |b txt  |2 rdacontent 
337 |a ƒaComputermedien  |b c  |2 rdamedia 
338 |a ƒa Online-Ressource  |b cr  |2 rdacarrier 
500 |a Date Completed 04.08.2008 
500 |a Date Revised 11.06.2008 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a A composite material comprising platinum nanoparticles supported on molecular sieve templated carbon was synthesized and found to adsorb 1.35 wt % hydrogen at 298 K and 100 atm. The isosteric heat of adsorption for the material at low coverage was approximately 14 kJ/mol, and it approached a value of 10.6 kJ/mol as coverage increased for pressures at and above 1 atm. The increase in capacity is attributed to spillover, which is observed with the use of isotopic tracer TPD. IRMOF-8 bridged to Pt/C, a material known to exhibit hydrogen spillover at room temperature, was also studied with the hydrogen-deuterium scrambling reaction for comparison. The isotherms were reversible. For desorption, sequential doses of H2 and D2 at room temperature and subsequent TPD yield product distributions that are strong indicators of the surface diffusion controlled reverse spillover process 
650 4 |a Journal Article 
700 1 |a Yang, Ralph T  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1992  |g 24(2008), 12 vom: 17. Juni, Seite 6159-65  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:24  |g year:2008  |g number:12  |g day:17  |g month:06  |g pages:6159-65 
856 4 0 |u http://dx.doi.org/10.1021/la800371j  |3 Volltext 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 24  |j 2008  |e 12  |b 17  |c 06  |h 6159-65