A 20 MHz single-element ultrasonic probe using 0.91Pb(Zn(1/3 )Nb(2/3))O(3)-0.09PbTiO(3) single crystal

A 20 MHz single-element ultrasonic probe using 0.91Pb(Zn(1/3 )Nb(2/3))O(3)-0.09PbTiO(3) (PZN-PT 91/9) single crystal has been fabricated. The single crystal of PZN-PT 91/9 orientated to the (001) plane has longitudinal coupling factor of k(33)>90%, which is much larger than the k(33)=70 to 80% of...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:IEEE transactions on ultrasonics, ferroelectrics, and frequency control. - 1986. - 45(1998), 4 vom: 15., Seite 1071-6
1. Verfasser: Saitoh, S (VerfasserIn)
Weitere Verfasser: Kobayashi, T, Harada, K, Shimanuki, S, Yamashita, Y
Format: Online-Aufsatz
Sprache:English
Veröffentlicht: 1998
Zugriff auf das übergeordnete Werk:IEEE transactions on ultrasonics, ferroelectrics, and frequency control
Schlagworte:Journal Article
Beschreibung
Zusammenfassung:A 20 MHz single-element ultrasonic probe using 0.91Pb(Zn(1/3 )Nb(2/3))O(3)-0.09PbTiO(3) (PZN-PT 91/9) single crystal has been fabricated. The single crystal of PZN-PT 91/9 orientated to the (001) plane has longitudinal coupling factor of k(33)>90%, which is much larger than the k(33)=70 to 80% of conventional Pb(Zr(1-x),Ti(x))O(3) (PZT) based ceramics. A single crystal of PZN-PT 91/9 without inclusion or crack has been grown with dimensions of about 25x15x5 mm by the self-flux method. Because mechanical strength in the fabrication of disk transducers orientated to the (001) plane was sufficiently strong, under the same conditions as are applied to conventional PZT ceramics, a piston single-element probe with a diameter of 2.0 mm and a frequency of 20 MHz was successfully fabricated. The bandwidth of the PZN-PT 91/9 probe was 13-26 MHz, which was 4 MHz broader than that of the conventional PZT probe
Beschreibung:Date Completed 02.10.2012
Date Revised 04.02.2008
published: Print
Citation Status PubMed-not-MEDLINE
ISSN:1525-8955
DOI:10.1109/58.710590