Temperature-reversible ultrathin films of N-isopropylacrylamide terpolymer adsorbed at the solid-liquid interface

This article describes the stability and reversibility of ultrathin films of N-isopropylacrylamide (NIPA)-vinylimidazole (VI)-poly(ethylene glycol) (PEG) graft terpolymer adsorbed at the solid-liquid interface upon temperature cycling from below to above its phase transition temperature. The coil-to...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1992. - 23(2007), 24 vom: 20. Nov., Seite 12159-66
1. Verfasser: Wan, Lei (VerfasserIn)
Weitere Verfasser: Bisht, Harender S, You, Ye-Zi, Oupicky, David, Mao, Guangzhao
Format: Aufsatz
Sprache:English
Veröffentlicht: 2007
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article Research Support, N.I.H., Extramural Research Support, Non-U.S. Gov't Research Support, U.S. Gov't, Non-P.H.S. Acrylic Resins Biocompatible Materials Water 059QF0KO0R poly-N-isopropylacrylamide 25189-55-3
LEADER 01000naa a22002652 4500
001 NLM174643780
003 DE-627
005 20231223140356.0
007 tu
008 231223s2007 xx ||||| 00| ||eng c
028 5 2 |a pubmed24n0582.xml 
035 |a (DE-627)NLM174643780 
035 |a (NLM)17963410 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Wan, Lei  |e verfasserin  |4 aut 
245 1 0 |a Temperature-reversible ultrathin films of N-isopropylacrylamide terpolymer adsorbed at the solid-liquid interface 
264 1 |c 2007 
336 |a Text  |b txt  |2 rdacontent 
337 |a ohne Hilfsmittel zu benutzen  |b n  |2 rdamedia 
338 |a Band  |b nc  |2 rdacarrier 
500 |a Date Completed 08.02.2008 
500 |a Date Revised 21.11.2013 
500 |a published: Print-Electronic 
500 |a Citation Status MEDLINE 
520 |a This article describes the stability and reversibility of ultrathin films of N-isopropylacrylamide (NIPA)-vinylimidazole (VI)-poly(ethylene glycol) (PEG) graft terpolymer adsorbed at the solid-liquid interface upon temperature cycling from below to above its phase transition temperature. The coil-to-globule and globule-to-coil phase transitions were captured by in situ fluid tapping atomic force microscopy (AFM). The film thickness of 1 nm was determined by AFM, X-ray photoelectron spectroscopy, and X-ray reflectivity. The concentration required to reach full coverage was found to be higher when adsorption occurred below the phase transition temperature. From 23 to 42 degrees C, the adsorbed NIPA terpolymer film was observed to be molecularly smooth, corresponding to the close-packed structure of flexible polymer coils. Particles containing between one and a few globules appeared abruptly at the interface at 42-43 degrees C, the same temperature as the solution phase transition temperature, which was determined by dynamic light scattering. The size of the particles did not change with temperature, whereas the number of particles increased with increasing temperature up to 60 degrees C. The particles correspond to the collapsed and associated state of the globules. The film morphological changes were found to be reversible upon temperature cycling. Subtle differences were observed between dip-coated and spin-coated films that are consistent with a higher degree of molecular freedom for spin-coated films. The study contributes to the fundamental understanding and applications of smart ultrathin films and coatings 
650 4 |a Journal Article 
650 4 |a Research Support, N.I.H., Extramural 
650 4 |a Research Support, Non-U.S. Gov't 
650 4 |a Research Support, U.S. Gov't, Non-P.H.S. 
650 7 |a Acrylic Resins  |2 NLM 
650 7 |a Biocompatible Materials  |2 NLM 
650 7 |a Water  |2 NLM 
650 7 |a 059QF0KO0R  |2 NLM 
650 7 |a poly-N-isopropylacrylamide  |2 NLM 
650 7 |a 25189-55-3  |2 NLM 
700 1 |a Bisht, Harender S  |e verfasserin  |4 aut 
700 1 |a You, Ye-Zi  |e verfasserin  |4 aut 
700 1 |a Oupicky, David  |e verfasserin  |4 aut 
700 1 |a Mao, Guangzhao  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1992  |g 23(2007), 24 vom: 20. Nov., Seite 12159-66  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:23  |g year:2007  |g number:24  |g day:20  |g month:11  |g pages:12159-66 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 23  |j 2007  |e 24  |b 20  |c 11  |h 12159-66