Corrosion studies and interfacial bonding of urea/poly(dimethylsiloxane) sol/gel hydrophobic coatings on AA 2024 aluminum alloy

Bis[(ureapropyl)triethoxysilane] bis(propyl)-terminated-polydimethylsiloxane 1000 (PDMSU), an organic-inorganic hybrid, diluted in either EtOH or a mixture of EtOH-PrOH, was used in thin film form (<200 nm) to inhibit the corrosion of AA 2024 alloy. Potentiodynamic, time-dependent cyclovoltammetr...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1992. - 23(2007), 10 vom: 08. Mai, Seite 5505-14
1. Verfasser: Fir, Mojca (VerfasserIn)
Weitere Verfasser: Orel, Boris, Vuk, Angela Surca, Vilcnik, Aljaz, Jese, Robi, Francetic, Vojmir
Format: Aufsatz
Sprache:English
Veröffentlicht: 2007
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article
LEADER 01000naa a22002652 4500
001 NLM169624005
003 DE-627
005 20231223121733.0
007 tu
008 231223s2007 xx ||||| 00| ||eng c
028 5 2 |a pubmed24n0566.xml 
035 |a (DE-627)NLM169624005 
035 |a (NLM)17429986 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Fir, Mojca  |e verfasserin  |4 aut 
245 1 0 |a Corrosion studies and interfacial bonding of urea/poly(dimethylsiloxane) sol/gel hydrophobic coatings on AA 2024 aluminum alloy 
264 1 |c 2007 
336 |a Text  |b txt  |2 rdacontent 
337 |a ohne Hilfsmittel zu benutzen  |b n  |2 rdamedia 
338 |a Band  |b nc  |2 rdacarrier 
500 |a Date Completed 27.06.2007 
500 |a Date Revised 01.05.2007 
500 |a published: Print-Electronic 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a Bis[(ureapropyl)triethoxysilane] bis(propyl)-terminated-polydimethylsiloxane 1000 (PDMSU), an organic-inorganic hybrid, diluted in either EtOH or a mixture of EtOH-PrOH, was used in thin film form (<200 nm) to inhibit the corrosion of AA 2024 alloy. Potentiodynamic, time-dependent cyclovoltammetric measurements and salt spray tests showed that the corrosion inhibition of the latter was 10 times higher than that of the former films. This was correlated with the higher degree of hydrolysis and the formation of more open polyhedral silsesquioxane species (T2) in the bulk heat-treated PDMSU/EtOH-PrOH xerogels (29Si NMR spectra). The structure of the coatings deposited on AA 2024 Al alloy was deduced from the infrared reflection-absorption (IR RA) spectra, which revealed more extensive urea-urea interactions and more efficient silane-Al interface bonding for the PDMSU/EtOH-PrOH coatings with higher corrosion inhibition. Ex situ IR RA potentiodynamic spectroelectrochemical measurements of PDMSU coatings revealed that their degradation did not proceed via the formation of silanol groups and consequent hydration of the coatings but that they decomposed above E(corr) by forming fragments composed of -CH2- segments in an all-trans conformation 
650 4 |a Journal Article 
700 1 |a Orel, Boris  |e verfasserin  |4 aut 
700 1 |a Vuk, Angela Surca  |e verfasserin  |4 aut 
700 1 |a Vilcnik, Aljaz  |e verfasserin  |4 aut 
700 1 |a Jese, Robi  |e verfasserin  |4 aut 
700 1 |a Francetic, Vojmir  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1992  |g 23(2007), 10 vom: 08. Mai, Seite 5505-14  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:23  |g year:2007  |g number:10  |g day:08  |g month:05  |g pages:5505-14 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 23  |j 2007  |e 10  |b 08  |c 05  |h 5505-14