Nanoscale hydrophobic recovery : A chemical force microscopy study of UV/ozone-treated cross-linked poly(dimethylsiloxane)

Chemical force microscopy (CFM) in water was used to map the surface hydrophobicity of UV/ozone-treated poly(dimethylsiloxane) (PDMS; Sylgard 184) as a function of the storage/recovery time. In addition to CFM pull-off force mapping, we applied indentation mapping to probe the changes in the normali...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Langmuir : the ACS journal of surfaces and colloids. - 1992. - 20(2004), 3 vom: 03. Feb., Seite 785-94
1. Verfasser: Hillborg, Henrik (VerfasserIn)
Weitere Verfasser: Tomczak, Nikodem, Olàh, Attila, Schönherr, Holger, Vancso, G Julius
Format: Aufsatz
Sprache:English
Veröffentlicht: 2004
Zugriff auf das übergeordnete Werk:Langmuir : the ACS journal of surfaces and colloids
Schlagworte:Journal Article
LEADER 01000naa a22002652 4500
001 NLM154266051
003 DE-627
005 20231223065649.0
007 tu
008 231223s2004 xx ||||| 00| ||eng c
028 5 2 |a pubmed24n0514.xml 
035 |a (DE-627)NLM154266051 
035 |a (NLM)15773106 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Hillborg, Henrik  |e verfasserin  |4 aut 
245 1 0 |a Nanoscale hydrophobic recovery  |b A chemical force microscopy study of UV/ozone-treated cross-linked poly(dimethylsiloxane) 
264 1 |c 2004 
336 |a Text  |b txt  |2 rdacontent 
337 |a ohne Hilfsmittel zu benutzen  |b n  |2 rdamedia 
338 |a Band  |b nc  |2 rdacarrier 
500 |a Date Completed 03.02.2006 
500 |a Date Revised 26.10.2019 
500 |a published: Print 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a Chemical force microscopy (CFM) in water was used to map the surface hydrophobicity of UV/ozone-treated poly(dimethylsiloxane) (PDMS; Sylgard 184) as a function of the storage/recovery time. In addition to CFM pull-off force mapping, we applied indentation mapping to probe the changes in the normalized modulus. These experiments were complemented by results on surface properties assessed on the micrometer scale by X-ray photoelectron spectroscopy and water contact-angle measurements. Exposure times of < or = 30 min resulted in laterally homogeneously oxidized surfaces, which are characterized by an increased modulus and a high segmental mobility of PDMS. As detected on a sub-50-nm level, the subsequent "hydrophobic recovery" was characterized by a gradual increase in the pull-off forces and a decrease in the normalized modulus, approaching the values of unexposed PDMS after 8-50 days. Lateral imaging on briefly exposed PDMS showed the appearance of liquid PDMS in the form of droplets with an increasing recovery time. Longer exposure times (60 min) led to the formation of a hydrophilic silica-like surface layer. Under these conditions, a gradual surface reconstruction within the silica-like layer occurred with time after exposure, where a hydrophilic SiOx-enriched phase formed < 100-nm-sized domains, surrounded by a more hydrophobic matrix with lower normalized modulus. These results provide new insights into the lateral homogeneity of oxidized PDMS with a resolution in the sub-50-nm range 
650 4 |a Journal Article 
700 1 |a Tomczak, Nikodem  |e verfasserin  |4 aut 
700 1 |a Olàh, Attila  |e verfasserin  |4 aut 
700 1 |a Schönherr, Holger  |e verfasserin  |4 aut 
700 1 |a Vancso, G Julius  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Langmuir : the ACS journal of surfaces and colloids  |d 1992  |g 20(2004), 3 vom: 03. Feb., Seite 785-94  |w (DE-627)NLM098181009  |x 1520-5827  |7 nnns 
773 1 8 |g volume:20  |g year:2004  |g number:3  |g day:03  |g month:02  |g pages:785-94 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_22 
912 |a GBV_ILN_350 
912 |a GBV_ILN_721 
951 |a AR 
952 |d 20  |j 2004  |e 3  |b 03  |c 02  |h 785-94