XANES study of Li-MgO and Li-La2O3-MgO catalysts for oxidative coupling of methane

To characterize the defect sites in the near-surface and bulk phase of Li-MgO and Li-La2O3-MgO, XANES at Mg K-edge and La L3-edge was applied. For Li-MgO, it can be suggested that Li doping at a low content (2.5 wt%) brings about the formation of defect species only in the near-surface. This is due...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Journal of synchrotron radiation. - 1994. - 8(2001), Pt 2 vom: 01. März, Seite 593-5
1. Verfasser: Aritani, H (VerfasserIn)
Weitere Verfasser: Yamada, H, Yamamoto, T, Tanaka, T, Imamura, S
Format: Aufsatz
Sprache:English
Veröffentlicht: 2001
Zugriff auf das übergeordnete Werk:Journal of synchrotron radiation
Schlagworte:Journal Article
LEADER 01000naa a22002652 4500
001 NLM114115575
003 DE-627
005 20231222165245.0
007 tu
008 231222s2001 xx ||||| 00| ||eng c
028 5 2 |a pubmed24n0381.xml 
035 |a (DE-627)NLM114115575 
035 |a (NLM)11512862 
040 |a DE-627  |b ger  |c DE-627  |e rakwb 
041 |a eng 
100 1 |a Aritani, H  |e verfasserin  |4 aut 
245 1 0 |a XANES study of Li-MgO and Li-La2O3-MgO catalysts for oxidative coupling of methane 
264 1 |c 2001 
336 |a Text  |b txt  |2 rdacontent 
337 |a ohne Hilfsmittel zu benutzen  |b n  |2 rdamedia 
338 |a Band  |b nc  |2 rdacarrier 
500 |a Date Completed 06.09.2001 
500 |a Date Revised 05.06.2019 
500 |a published: Print 
500 |a Citation Status PubMed-not-MEDLINE 
520 |a To characterize the defect sites in the near-surface and bulk phase of Li-MgO and Li-La2O3-MgO, XANES at Mg K-edge and La L3-edge was applied. For Li-MgO, it can be suggested that Li doping at a low content (2.5 wt%) brings about the formation of defect species only in the near-surface. This is due to the localization of doped Li ions in the surface, and thus the catalytically active species containing [Li+ O-] type center exist in the surface region. After OCM reaction, the detect species are formed in the near-surface over MgO and Li-MgO. By addition of La2O3 to Li-MgO (La/(Mg+La)=0.25), the structural change during the reaction is almost suppressed in the surface. In addition, the Li-La2O3-MgO shows higher C2 selectivity than Li-MgO 
650 4 |a Journal Article 
700 1 |a Yamada, H  |e verfasserin  |4 aut 
700 1 |a Yamamoto, T  |e verfasserin  |4 aut 
700 1 |a Tanaka, T  |e verfasserin  |4 aut 
700 1 |a Imamura, S  |e verfasserin  |4 aut 
773 0 8 |i Enthalten in  |t Journal of synchrotron radiation  |d 1994  |g 8(2001), Pt 2 vom: 01. März, Seite 593-5  |w (DE-627)NLM09824129X  |x 1600-5775  |7 nnns 
773 1 8 |g volume:8  |g year:2001  |g number:Pt 2  |g day:01  |g month:03  |g pages:593-5 
912 |a GBV_USEFLAG_A 
912 |a SYSFLAG_A 
912 |a GBV_NLM 
912 |a GBV_ILN_40 
912 |a GBV_ILN_350 
912 |a GBV_ILN_2005 
951 |a AR 
952 |d 8  |j 2001  |e Pt 2  |b 01  |c 03  |h 593-5