APA Zitierstil

Guo, Y., Pan, S., Yi, X., Chi, S., Yin, X., Geng, C., . . . Yang, Q. (2024). Fluorinating All Interfaces Enables Super-Stable Solid-State Lithium Batteries by In Situ Conversion of Detrimental Surface Li2CO3. Advanced materials (Deerfield Beach, Fla.), 36(13), . https://doi.org/10.1002/adma.202308493

Chicago Zitierstil

Guo, Yong, et al. "Fluorinating All Interfaces Enables Super-Stable Solid-State Lithium Batteries by In Situ Conversion of Detrimental Surface Li2CO3." Advanced Materials (Deerfield Beach, Fla.) 36, no. 13 (2024). https://dx.doi.org/10.1002/adma.202308493.

MLA Zitierstil

Guo, Yong, et al. "Fluorinating All Interfaces Enables Super-Stable Solid-State Lithium Batteries by In Situ Conversion of Detrimental Surface Li2CO3." Advanced Materials (Deerfield Beach, Fla.), vol. 36, no. 13, 2024.